Wang X, Hu Y, Song L, Yang HY, Xing WY, Lu HD (2011b) Progress in Organic Coatings 71(1), 72-82.
文章来源:WOS    作者:SKLFS    发布时间:2011-08-16

Wang X, Hu Y, Song L, Yang HY, Xing WY, Lu HD (2011b) Synthesis and characterization of a DOPO-substitued organophosphorus oligomer and its application in flame retardant epoxy resins. Progress in Organic Coatings 71(1), 72-82. [In English]

Web link: http://dx.doi.org/10.1016/j.porgcoat.2010.12.013

Keywords:

Epoxy resins; Flame retardancy; Organophosphorus oligomer; Thermal; degradation; thermal-degradation; cured products; curing agent; phosphorus; behavior; composites

Abstract: Advanced flame retardant epoxy resins with different contents of poly(DOPO substituted phenyl dimethanol pentaerythritol diphosphonate) (PFR) were prepared. PER was synthesized from the polycondensation of DOPO-disubstituted benzenedimethanol (TDCA-DOPO) with pentaerythritol diphosphonate dichloride (SPDPC). The flame retardancy and thermal stability of the EP/PFR hybrids were investigated by limiting oxygen index (LOI), UL-94 test and thermogravimetric analysis (TGA) in air. LOI values increased from 21.5 for pure EP to 36.0 for phosphorus-containing resins, and UL-94 V-O materials were obtained with the 15 wt% PER. The TGA results indicated that incorporation of PFR significantly enhanced the char yield and the thermal stability of char layer at higher temperature. Differential scanning calorimetry revealed that the EP/PFR composites possessed higher glass transition temperatures than phosphorus-free EP, which was consistent with dynamic mechanical analysis results. The thermal degradation behaviors of the EP/PFR composites were investigated by real time Fourier transform infrared spectra (RTFTIR), thermogravimetric analysis/infrared spectrometry (TG-IR) and direct pyrolysis/mass (DP-MS) analysis. The results suggested that the addition of PER can reduce the release of combustible gas, trap the H and OH radicals by releasing the PO radical and induce the formation of char layer, thus retard the polymer degradation and combustion process. (C) 2011 Elsevier B.V. All rights reserved.

 
 
相关链接
Wang X, Hu Y, Song L, Yang HY, Xing WY, Lu HD (2011b) Progress in Organic Coatings 71(1), 72-82.
联系我们
安徽省合肥市金寨路96号
图书馆VIP
火灾科学国家重点实验室
邮政编码:230026
   
Tel:(+86)551 63601651
Fax:(+86)551 63601669
E-mail:sklfs@ustc.tsg211.com
Copyright © 1990-2011 State Key Laboratory of Fire Science, University of Science and Technology of China
火灾科学国家重点实验室 版权所有 皖ICP备:002106505 号